Please contact us to tell us your details requirements, our sales person will give you professional suggestion and make the PI.
30% T/T deposit, 70% balance payment against BL Copy. We also accept 100% L/C at sight and DP payment.
1x20gp or 1x40hq container based on dangerous cargoes. If you have another container shipped out from China, we accept small quantities and send them to your other supplier's warehouse and load them together.
3 years warranty, you can contact us if you have any questions during the warranty period!
If you got damage products, please show us the photo/video and quantity, we will send you the same quantity for your next order for free.
You can choose color from our color chart, or customize based on RAL color / Pantone Color. Or you can provide your color sample.
Yes, you can make your own design. If you don’t have a design, you can send us a logo file and tell us what you want, and our designers will help you design it for free.
Yes, Chinese color sticker, English color sticker, Spanish color sticker, Russian color sticker, Hebrew color sticker,color sticker without text, etc. We can also customize according to your needs.
About Company
These contents can help you know our company. If you have any questions, please feel free to contact us.
Our company was established in 2006, more than 18 years.
Around 550 employee.
Our company is recognized by numerous quality control systems including ISO9001, SGS, CNAS, SMQ, and QCQ.
The daily production capacity is approximately 500,000pcs perday, 150 million pieces per year.
Our company has an R&D center and a professional technical team of more than 50 people.
Construction issues
When your customers encounter these problems during construction, you can teach them how to solve them.
Reasons:
Grease, watermarks, or dirt on the base material
Base metal surface too rough or unpolished
Aging, powdering, or cracking of old primer
How to Use:
Thoroughly clean the surface
Sand the metal surface
Remove the aged paint and reapply the surface paint
Reasons:
1. Surface contamination with oil, wax, water, or dust
2. Excessive humidity in the environment
How to Use:
1. Thoroughly clean and dry the surface
2. Sand the metal surface
3. Reapply the paint
Reasons:
1. Mismatch between primer and topcoat in flexibility and rigidity
2. Applying topcoat before primer is dry
3. The topcoat was applied too thickly
4. Aging, powdering, and cracking of old primer
How to Use:
1. Ensure primer and topcoat are compatible; use a middle coat if necessary.
2. Remove the aged primer and reapply topcoat.
Reasons:
1. Paint coat applied too thickly
2. Poor drying conditions, such as low temperature, high humidity, or excessive ventilation
3. Contaminated air or poor ventilation
How to Use:
1. Avoid applying the paint too thickly
2. Ensure fresh air, normal temperature, and proper humidity in the spraying environment
Reasons:
1. High humidity (≥80%)
2. Very cold weather
How to Use:
Avoid spraying in rainy, humid, or extreme temperatures
Reasons:
1. Spray nozzle too close to the surface
2. Moving the spray nozzle too slowly
3. Poor ventilation
4. Insufficient drying time between layers
5. Inadequate surface cleaning
How to Use:
1. Maintain a proper spraying distance (15-25 cm)
2. Move the spray nozzle at a normal speed (30-60 cm/s)
3. Ensure good ventilation
4. Allow appropriate drying time between layers (3-10 min, depending on temperature)
5. Thoroughly clean the surface before spraying